发布网友 发布时间:2022-10-08 08:08
共2个回答
热心网友 时间:2023-11-07 19:32
Abstract: ferrous ammonium sulfate hexahydrate, ammonium dihydrogen phosphate, lithium hydroxide as raw material, the use of liquid coprecipitation LiFePO_4 material. Lithium hydroxide: ammonium dihydrogen phosphate: the amount of ferrous ammonium sulfate hexahydrate ratio of 3:1:1.. , feed concentration was 0. 1mol / L, reaction temperature is 60 ℃, reaction time was 45 min, heat treatment, the temperature is 700 ℃, handling about 8 h. Were carried out using XRD characterization, then the nature of its battery of tests.热心网友 时间:2023-11-07 19:32
With ferrous ammonium sulfate hexahydrate, ammonium dihydrogen phosphate, lithium hydroxide as raw materials by liquid coprecipitation LiFePO_4 material. Lithium hydroxide: ammonium dihydrogen phosphate: the amount of ferrous ammonium sulfate hexahydrate ratio of 3:1:1.. , feed concentration was 0. 1mol / L, reaction temperature is 60 ℃, reaction time was 45 min, heat treatment, the temperature is 700 ℃, handling about 8 h. Were carried out using XRD characterization, then the nature of its battery of tests.